==Which glass should I use to make beads from?==
 
==Which glass should I use to make beads from?==
  
*[[Plowden and Thompson]] (English)  
+
*[[Plowden and Thompson]] (English COE 100 and 93)  
*[[Effetre]] (Italian)  
+
*[[Effetre]] (Italian COE 104)  
*[[Bullseye]] (American)  
+
*[[Bullseye]] (American COE 90)  
*[[Satake]] (Japanese)  
+
*[[Satake]] (Japanese COE 120)  
*[[Reichenbach]] (German)
+
*[[Reichenbach]] (German COE 104 and 96)
*[[ASK]]
+
*[[Lauscha]] (German COE 104)
*[[Lauscha]]  
+
*[[CiM]] (American COE 104)
*[[CiM]]
+
*[[Northstar]] (American COE 104)
*[[Northstar]]
+
*[[Double Helix]] (American COE 104)
*[[Double Helix]]
+
*[[Vetrofond]] (Italian COE 104)
*[[Vetrofond]]
+
*[[Kugler]] (German COE 104 and 96)
 +
*[[Gaffer]] (New Zealand COE 96)
 +
*[[TAG 104]] (American COE 104)
 +
*[[Clear Glass]]
  
===Other glass rod manufacturers===
+
===[[Borosilicate Glass]]===
  
 +
*[[TAG 33]] (American)
 +
*[[Northstar 33]] (American)
 +
*[[Glass Alchemy]] (American)
 +
*[[Momka]] (American)
 +
*[[Borostix]] (American)
  
 
===Using sheet art glass===
 
===Using sheet art glass===

Latest revision as of 07:13, 14 November 2012

Which glass should I use to make beads from?

Borosilicate Glass

Using sheet art glass

Scrap glass from bottles etc.

Further information

See http://www.glass-beads.co.uk/Flame/June06/WhichGlass.html for more information