Glass: Difference between revisions
Appearance
| (10 intermediate revisions by 5 users not shown) | |||
| Line 1: | Line 1: | ||
==Which glass should I use to make beads from?== | ==Which glass should I use to make beads from?== | ||
[[Plowden and Thompson]] (English) | *[[Plowden and Thompson]] (English COE 100 and 93) | ||
*[[Effetre]] (Italian COE 104) | |||
*[[Bullseye]] (American COE 90) | |||
*[[Satake]] (Japanese COE 120) | |||
*[[Reichenbach]] (German COE 104 and 96) | |||
*[[Lauscha]] (German COE 104) | |||
*[[CiM]] (American COE 104) | |||
*[[Northstar]] (American COE 104) | |||
*[[Double Helix]] (American COE 104) | |||
*[[Vetrofond]] (Italian COE 104) | |||
*[[Kugler]] (German COE 104 and 96) | |||
*[[Gaffer]] (New Zealand COE 96) | |||
*[[TAG 104]] (American COE 104) | |||
*[[Clear Glass]] | |||
[[ | ===[[Borosilicate Glass]]=== | ||
[[ | *[[TAG 33]] (American) | ||
*[[Northstar 33]] (American) | |||
*[[Glass Alchemy]] (American) | |||
*[[Momka]] (American) | |||
*[[Borostix]] (American) | |||
===Using sheet art glass=== | |||
===Scrap glass from bottles etc.=== | ===Scrap glass from bottles etc.=== | ||
== Further information == | |||
See http://www.glass-beads.co.uk/Flame/June06/WhichGlass.html for more information | See http://www.glass-beads.co.uk/Flame/June06/WhichGlass.html for more information | ||
Latest revision as of 13:13, 14 November 2012
Which glass should I use to make beads from?
- Plowden and Thompson (English COE 100 and 93)
- Effetre (Italian COE 104)
- Bullseye (American COE 90)
- Satake (Japanese COE 120)
- Reichenbach (German COE 104 and 96)
- Lauscha (German COE 104)
- CiM (American COE 104)
- Northstar (American COE 104)
- Double Helix (American COE 104)
- Vetrofond (Italian COE 104)
- Kugler (German COE 104 and 96)
- Gaffer (New Zealand COE 96)
- TAG 104 (American COE 104)
- Clear Glass
- TAG 33 (American)
- Northstar 33 (American)
- Glass Alchemy (American)
- Momka (American)
- Borostix (American)
Using sheet art glass
Scrap glass from bottles etc.
Further information
See http://www.glass-beads.co.uk/Flame/June06/WhichGlass.html for more information