Jump to content

Amber/purple

From Fritipedia
Revision as of 12:04, 23 September 2010 by Garishglobes (talk | contribs) (New page: The term 'amber/purple' generally refers to glass that absorbs amber light and reflects purples - in a dull room, the glass will appear amber coloured, but with good light, or in bright su...)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

The term 'amber/purple' generally refers to glass that absorbs amber light and reflects purples - in a dull room, the glass will appear amber coloured, but with good light, or in bright sunlight, a range of colours will be reflected, in particular blues and purples.