Revision as of 00:33, 15 November 2008 by Jolene (talk | contribs) (New page: Northstar Glassworks INC produce boro glass rods for lampwork. They currently have 116 boro colours in their pallette. Northstar also have a small but beautiful range of silver ric...)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigationJump to search

Northstar Glassworks INC produce boro glass rods for lampwork. They currently have 116 boro colours in their pallette. Northstar also have a small but beautiful range of silver rich glass rods that are CoE 104. These are sold under the name Precision 104