Vetrofond
From Fritipedia
Revision as of 08:55, 14 November 2008 by Jolene (talk | contribs) (New page: Vetrofond glass is manufactured in Italy Vetrofond colours and stock numbers Transparent 1004 clear 1005 crystal clear 1008 yellow 1012 light topaz 1014 [...)
Vetrofond glass is manufactured in Italy
Vetrofond colours and stock numbers
Transparent 1004 clear 1005 crystal clear 1008 yellow 1012 light topaz 1014 topaz 1020 light grass green 1022 grass green 1024 dark grass green 1026 teal 1028 light emerald green