Vetrofond glass is manufactured in Italy. Many stockists of Vetrofond glass rods use their own colour descriptions and stock numbers. The last 4 digits used by any stockist for their stock numbers will refer to the Vetrofond factory stock number.
Vetrofond colours and stock numbers
Transparent
Stock Number
|
Colour
|
Properties
|
Reactions
|
1004
|
clear
|
colours appear lighter encased in clear
|
|
1005
|
crystal clear
|
good for encasing silver glass
|
|
1008
|
yellow
|
|
|
1012
|
light topaz
|
|
|
1014
|
topaz
|
|
reacts with silver glass - reacts with silver to produce organic effects
|
1020
|
light grass green
|
|
reacts with silver glass
|
1022
|
grass green
|
|
|
1024
|
dark grass green
|
|
|
1026
|
teal
|
|
|
1028
|
light emerald green
|
|
|
1030
|
emerald green
|
|
|
1034
|
light aquamarine
|
|
|
1036
|
aquamarine (aqua)
|
|
|
1038
|
pale aquamarine (light aqua)
|
|
|
1040
|
light purple
|
|
|
1042
|
purple
|
|
|
1044
|
dark purple
|
|
|
1048
|
grey
|
|
|
1052
|
light blue
|
|
|
1054
|
blue
|
|
|
1058
|
intense blue
|
|
|
1060
|
cobalt blue
|
|
|
1064
|
black
|
|
|
1068
|
pink
|
|
|
1069
|
electric yellow
|
striking
|
|
1072
|
orange
|
striking
|
|
1076
|
red
|
|
|
1080
|
pale lavender
|
|
|
1082
|
lavender blue (alexandrite)
|
|
|
1084
|
light brown
|
|
|
1086
|
medium brown
|
|
|
1088
|
dark brown
|
|
|
Opaque/pastels
Stock Number
|
Colour
|
Properties
|
Reactions
|
1204
|
white
|
melts easily
|
|
1206
|
anice white
|
very shocky
|
reacts with [Effetre]] nero intenso
|
1208
|
silk white
|
|
|
1212
|
pea green
|
|
reduces in a propane rich flame
|
1214
|
nile green
|
|
|
1216
|
grass green
|
|
|
1218
|
dark grass green
|
very shocky
|
|
1220
|
periwinkle
|
|
|
1224
|
light sky blue
|
|
reduces in a propane rich flame
|
1228
|
dark sky blue
|
|
reduces in a propane rich flame
|
1232
|
turquoise
|
|
reduces in a propane rich flame - reacts with ivory
|
1236
|
dark turquoise
|
|
reduces in a propane rich flame - reacts with ivory
|
1240
|
light lapis blue
|
|
|
1242
|
lapis blue
|
|
|
1246
|
cobalt blue
|
|
|
1248
|
light grey
|
|
|
1250
|
medium grey
|
|
|
1255
|
flower pink
|
|
|
1262
|
dark ivory
|
|
reacts with fine silver to produce organic effects - reacts with copper glass
|
1264
|
light ivory
|
|
reacts with fine silver to produce organic effects - reacts with copper glass
|
1268
|
pearl grey
|
|
|
1272
|
violet
|
|
|
Specials
Stock Number
|
Colour
|
Properties
|
Reactions
|
1408
|
medium yellow
|
|
|
1412
|
dark lemon
|
|
|
1420
|
coral
|
|
|
1424
|
carrot red
|
|
|
1428
|
light red
|
|
|
1432
|
medium red
|
|
|
1438
|
red purple
|
|
|
1444
|
light brown
|
|
|
448
|
dark brown
|
|
|
1456
|
gold pink
|
|
|
1460
|
yellow ocher (wasabi)
|
|
|
Odd lots
Stock Number
|
Colour
|
Properties
|
Reactions
|
1801
|
cosmic storm
|
|
reacts with silver glass - bleeds in to ivory glass
|
1802
|
apricot jam
|
|
|
1803
|
candy corn
|
|
|
1804
|
tomato soup
|
|
|
1805
|
orange dreamsicle
|
|
Reacts with [EDP]
|
1806
|
smoke rings
|
semi-transparent
|
|
1807
|
frog pond
|
|
|
1808
|
swamp moss
|
|
|
1809
|
jungle twilight
|
|
|
1810
|
lemongrass
|
semi-transparent
|
reacts with iris gold frit
|
1811
|
moon rock
|
striking
|
strikes from brick red to purplish coral
|
1906
|
chardonnay
|
|
|
1909
|
transparent green odd
|
|
|
1910
|
transparent yellow odd
|
|
|
1911
|
silk white (opal white)
|
|
|
1912
|
olive green pastel
|
|
|
1917
|
Transparent amber (streaky amber)
|
|
reacts with silver glass - reacts with ivory
|
1919
|
pale ivory
|
|
reacts with fine silver to produce organic effects
|
1922
|
transparent sage green
|
|
|
1925
|
transparent pale blue
|
|
|
1926
|
sea green (seafoam)
|
|
|
1927
|
ocean green
|
|
|
1931
|
river rock (brie)(avocado)
|
|
reacts with fine silver to produce organic effects
|
1932
|
fish pink
|
|
|
1933
|
pink no.3
|
|
|
1934
|
pink flower
|
|
|
1937
|
arancio perfecto
|
|
|
1938
|
pale aqua streaky
|
|
|
1939
|
intense tangerine
|
|
|
1943
|
orange sherbert
|
aka. free range salmon pink
|
reacts with silver glass
|
1940
|
italian marble
|
|
|
1941
|
pineapple yellow
|
|
|
1942
|
watermelon (poppy)
|
|
reacts with silver glass - reacts with ivory and fine silver
|
1944
|
tangerine
|
|
|
1945
|
new white (custard)
|
|
|
1946
|
sunshine 1947 yellow ice (lemon ice)(belgian lace)
|
|
|
1948
|
banana cream
|
|
|
1949
|
lemon meringue
|
|
reacts with Effetre copper green
|
1951
|
transparent candy apple red
|
|
|
1952
|
violet odd (purplicious)
|
|
reacts with fine silver and also ivory to produce organic effects
|
1954
|
cool white (odd cotton)
|
|
reacts with fine silver
|
1955
|
seashell swirl
|
|
reacts with fine silver and ivory
|
1957
|
orange punch
|
|
|
1958
|
pyjama blue
|
|
|
1960
|
light pink
|
|
|
1961
|
carrot red
|
this glass contains sparkles
|
|
1963
|
green tepenade
|
|
|
1964
|
pale avocado
|
|
|
1965
|
olive green
|
|
|
1966
|
dark olive green
|
|
|
1967
|
quartz grey
|
|
|
1968
|
slate blue
|
|
|
1969
|
pearl grey
|
|
|
1970
|
transparent streaky sapphire
|
|
|
1975
|
midnight blue
|
black rod with a blue core
|
|
1976
|
key lime green
|
|
|
1977
|
parrot green
|
|
|
1978
|
transparent crystal green
|
striking
|
strikes to neon yellow
|
1980
|
light streaky brown
|
|
|
1981
|
streaky brown
|
|
|
1982
|
dark streaky brown
|
|
|
1983
|
pale ocean blue
|
|
|
1984
|
pale moss agate
|
|
reacts with silver glass
|
1985
|
moss agate
|
|
|
1986
|
lichen
|
|
reacts with fine silver and ivory
|
1987
|
dark lichen
|
|
reacts with fine silver and ivory
|
1988
|
pale crystal green
|
|
|
1989
|
transparent odd topaz
|
|
reacts with silver glass
|
1990
|
honey crunch
|
|
reacts with fine silver and silver glass
|
1991
|
marbled avocado
|
|
reacts with fine silver and silver glass
|
1992
|
banana
|
|
|
1993
|
sweet lime (red jasper)
|
|
reacts with fine silver and silver glass
|
1994
|
strawberry sweet (dark red jasper)
|
|
reacts with fine silver and silver glass
|
1995
|
jupiter
|
|
reacts with fine silver and silver glass
|
1996
|
bloody mary
|
|
reacts with fine silver and silver glass
|
1997
|
painted desert
|
striking
|
|
1998
|
rhubarb
|
|
reacts with fine silver and ivory glass
|
1999
|
petrified wood
|
|
reacts with fine silver and ivory glass
|