Vetrofond glass is manufactured in Italy. Many stockists of Vetrofond glass rods use their own colour descriptions and stock numbers. The last 4 digits used by any stockist for their stock numbers will refer to the Vetrofond factory stock number.
Vetrofond colours and stock numbers
Transparent
Colour
|
Properties
|
Reactions
|
1004 clear
|
Colours appear lighter encased in clear
|
|
1005 crystal clear
|
good for encasing silver glass
|
|
1008 yellow
|
|
|
1012 light topaz
|
|
|
1014 topaz
|
|
Reacts with DH psyche to give purples and blues
|
1020 light grass green
|
|
|
1022 grass green
|
|
|
1024 dark grass green
|
|
|
1026 teal
|
|
|
1028 light emerald green
|
|
|
1030 emerald green
|
|
|
1034 light aquamarine
|
|
|
1036 aquamarine (aqua)
|
|
|
1038 pale aquamarine (light aqua)
|
|
|
1040 light purple
|
|
|
1042 purple
|
|
|
1044 dark purple
|
|
|
1048 grey
|
|
|
1052 light blue
|
|
|
1054 blue
|
|
|
1058 intense blue
|
|
|
1060 cobalt blue
|
|
|
1064 black
|
|
|
1068 pink
|
|
|
1069 electric yellow
|
|
|
1072 orange
|
|
|
1076 red
|
|
|
1080 pale lavender
|
|
|
1082 lavender blue (alexandrite)
|
|
|
1084 light brown
|
|
|
1086 medium brown
|
|
|
1088 dark brown
|
|
|
Opaque/pastels
Colour
|
Properties
|
Reactions
|
1204 white
|
|
|
1206 anice white
|
|
|
1208 silk white
|
|
|
1212 pea green
|
|
|
1214 nile green
|
|
|
1216 grass green
|
|
|
1218 dark grass green
|
|
|
1220 periwinkle
|
|
|
1224 light sky blue
|
|
|
1228 dark sky blue
|
|
|
1232 turquoise
|
|
|
1236 dark turquoise
|
|
|
1240 light lapis blue
|
|
|
1242 lapis blue
|
|
|
1246 cobalt blue
|
|
|
1248 light grey
|
|
|
1250 medium grey
|
|
|
1255 flower pink
|
|
|
1262 dark ivory
|
|
|
1264 light ivory
|
|
|
1268 pearl grey
|
|
|
1272 violet
|
|
|
Specials
Colour
|
Properties
|
Reactions
|
1408 medium yellow
|
|
|
1412 dark lemon
|
|
|
1420 coral
|
|
|
1424 carrot red
|
|
|
1428 light red
|
|
|
1432 medium red
|
|
|
1438 red purple
|
|
|
1444 light brown
|
|
|
448 dark brown
|
|
|
1456 gold pink
|
|
|
1460 yellow ocher (wasabi)
|
|
|
Odd lots
Colour
|
Properties
|
Reactions
|
1801 cosmic storm
|
|
|
1802 apricot jam
|
|
|
1803 candy corn
|
|
|
1804 tomato soup
|
|
|
1805 orange dreamsicle
|
|
|
1806 smoke rings
|
|
|
1807 frog pond
|
|
|
1808 swamp moss
|
|
|
1809 jungle twilight
|
|
|
1810 lemongrass
|
|
|
1811 moon rock
|
|
|
1906 chardonnay
|
|
|
1909 transparent green odd
|
|
|
1910 transparent yellow odd
|
|
|
1911 silk white (opal white)
|
|
|
1912 olive green pastel
|
|
|
1917 Transparent amber (streaky amber)(antique amber)
|
|
|
1919 pale ivory
|
|
|
1922 transparent sage green
|
|
|
1925 transparent pale blue
|
|
|
1926 sea green (seafoam)
|
|
|
1927 ocean green
|
|
|
1931 river rock (brie)(avocado)
|
|
|
1932 fish pink
|
|
|
1933 pink no.3
|
|
|
1934 pink flower
|
|
|
1937 arancio perfecto
|
|
|
1938 pale aqua streaky
|
|
|
1939 intense tangerine
|
|
|
1943 orange sherbert (free range salmon pink)
|
|
|
1940 italian marble
|
|
|
1941 pineapple yellow
|
|
|
1942 watermelon (poppy)
|
|
|
1944 tangerine
|
|
|
1945 new white (custard)
|
|
|
1946 sunshine 1947 yellow ice (lemon ice)(belgian lace)
|
|
|
1948 banana cream
|
|
|
1949 lemon meringue
|
|
|
1951 transparent candy apple red
|
|
|
1952 violet odd (purplicious)
|
|
|
1954 cool white (odd cotton)
|
|
|
1955 seashell swirl
|
|
|
1957 orange punch
|
|
|
1958 pyjama blue
|
|
|
1960 light pink
|
|
|
1961 carrot red
|
|
|
1963 green tepenade
|
|
|
1964 pale avocado
|
|
|
1965 olive green
|
|
|
1966 dark olive green
|
|
|
1967 quartz grey
|
|
|
1968 slate blue
|
|
|
1969 pearl grey
|
|
|
1970 transparent streaky sapphire
|
|
|
1975 midnight blue
|
|
|
1976 key lime green
|
|
|
1977 parrot green
|
|
|
1978 transparent crystal green
|
|
|
1980 light streaky brown
|
|
|
1981 streaky brown
|
|
|
1982 dark streaky brown
|
|
|
1983 pale ocean blue
|
|
|
1984 pale moss agate
|
|
|
1985 moss agate
|
|
|
1986 lichen
|
|
|
1987 dark lichen
|
|
|
1988 pale crystal green
|
|
|
1989 transparent odd topaz
|
|
|
1990 honey crunch
|
|
|
1991 marbled avocado
|
|
|
1992 banana
|
|
|
1993 sweet lime (red jasper)
|
|
|
1994 strawberry sweet (dark red jasper)
|
|
|