Reichenback produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenback 104 glasses on a base bead of a very soft opaque colour (for example Effetre White) have a "bleed" effect rather than a crisp edge when melted down.