Difference between revisions of "Stringer"

From Fritipedia
Jump to navigationJump to search
(New page: Getting detail onto glass beads can often involve the use of stringer. Stringer can be made by the artist or bought commercially. Stringer can be used to get lines and dots on beads as wel...)
 
 
Line 1: Line 1:
Getting detail onto glass beads can often involve the use of stringer. Stringer can be made by the artist or bought commercially. Stringer can be used to get lines and dots on beads as well as being used to form twists / swirls in beads.  
+
Stringer are thin strands of [[glass]] often made by pulling molten [[glass]] until it forms a thin rod. Stringer can be made as thin as desired.
 +
 
 +
===Why do I need to use stringer?===
 +
Getting detail onto [[glass beads]] can often involve the use of stringer. Stringer can be made by the artist or bought commercially. Stringer can be used to get lines and dots on beads as well as being used to form [[twists]] or swirls in beads.
 +
 
===How is stringer made?===
 
===How is stringer made?===
Choose the rod of glass that you want to use as stringer and heat the end of the rod to form a [[gather]]. once the gather has formed allow the glass to begin cooling and then use tweezers to grip the end of the gather and pull. The faster you pull the thinner your stringer will be, if you want a thick stringer allow the glass to cool quite a bit and pull slowly. The stringer can then be broken off from the rod and used in designs later on.  
+
Choose the rod of [[glass]] that you want to use as stringer and heat the end of the rod to form a [[gather]]. Once the gather has formed, allow the glass to begin cooling slightly, then use tweezers to grip the end of the gather and pull. The faster you pull the thinner your stringer will be, if you want a thick stringer allow the glass to cool quite a bit and pull slowly. The stringer can then be broken off from the rod and used in designs later on.  
  
 
===Stringer control===  
 
===Stringer control===  
 
This takes practice!!!
 
This takes practice!!!

Latest revision as of 16:57, 20 November 2008

Stringer are thin strands of glass often made by pulling molten glass until it forms a thin rod. Stringer can be made as thin as desired.

Why do I need to use stringer?

Getting detail onto glass beads can often involve the use of stringer. Stringer can be made by the artist or bought commercially. Stringer can be used to get lines and dots on beads as well as being used to form twists or swirls in beads.

How is stringer made?

Choose the rod of glass that you want to use as stringer and heat the end of the rod to form a gather. Once the gather has formed, allow the glass to begin cooling slightly, then use tweezers to grip the end of the gather and pull. The faster you pull the thinner your stringer will be, if you want a thick stringer allow the glass to cool quite a bit and pull slowly. The stringer can then be broken off from the rod and used in designs later on.

Stringer control

This takes practice!!!