Jump to navigationJump to search (New page: ==What is soft glass?== Soft glass is glass that has a relatively low softening point, for example Effetre) |
|||
(2 intermediate revisions by 2 users not shown) | |||
Line 1: | Line 1: | ||
==What is soft glass?== | ==What is soft glass?== | ||
− | Soft glass is glass that has a relatively low softening point, for example [[Effetre]] | + | Soft glass is glass that has a relatively low softening point, for example [[Effetre]] or [[Vetrofond]]. Soft glass is sometimes also called soda lime glass. |