Difference between revisions of "Glass Masking"

From Fritipedia
Jump to navigationJump to search
(Created page with 'Start with a base colour (black) and put on a set of contrast dots (white) framed|none Add a further set of base colour (black) in between the wh...')
 
 
(6 intermediate revisions by the same user not shown)
Line 2: Line 2:
  
 
[[Image:Glass_Masking_01.png|framed|none]]
 
[[Image:Glass_Masking_01.png|framed|none]]
 +
 +
This is what it looks like on a bead
 +
 +
[[image:Step 1 Round black bead with white dots added.jpg|600px]]
 +
 +
And melted in:
 +
 +
[[image:Step 2 Round black bead with melted white dots.jpg|600px]]
  
 
Add a further set of base colour (black) in between the white dots.
 
Add a further set of base colour (black) in between the white dots.
Line 8: Line 16:
  
 
[[Image:Glass_Masking_02.png|framed|none]]
 
[[Image:Glass_Masking_02.png|framed|none]]
 +
 +
This is what it looks like on a bead
 +
 +
[[image:Step 3 Black dots between white dots being melted.jpg|600px]]
  
 
Repeat this with dots in between each of the white dots
 
Repeat this with dots in between each of the white dots
Line 18: Line 30:
  
 
[[Image:Glass_Masking_04.png|framed|none]]
 
[[Image:Glass_Masking_04.png|framed|none]]
 +
 +
And on an actual bead melted in:
 +
 +
[[image:Step 4 Black dots melted in.jpg|600px]]
  
 
Add a white dot (using a stringer) on top of each of the black dots
 
Add a white dot (using a stringer) on top of each of the black dots
  
 
[[Image:Glass_Masking_05.png|framed|none]]
 
[[Image:Glass_Masking_05.png|framed|none]]
 +
 +
This is what it looks like on a bead
 +
 +
[[image:Step 5 Black dots on White dots.jpg|600px]]
 +
 +
And melted in:
 +
 +
[[image:Step 6 Melted In.jpg|600px]]
  
 
Add a black dot (using a stringer) on top of each of the white dots
 
Add a black dot (using a stringer) on top of each of the white dots
Line 36: Line 60:
  
 
Add a small black dot (using a stringer) between each of the original large white dots
 
Add a small black dot (using a stringer) between each of the original large white dots
 +
 +
This is what it looks like on a bead
 +
 +
[[image:Step 7 More black dots.jpg|600px]]
  
 
Stop, when you feel you have done enough
 
Stop, when you feel you have done enough

Latest revision as of 15:30, 19 November 2012

Start with a base colour (black) and put on a set of contrast dots (white)

Glass Masking 01.png

This is what it looks like on a bead

Step 1 Round black bead with white dots added.jpg

And melted in:

Step 2 Round black bead with melted white dots.jpg

Add a further set of base colour (black) in between the white dots.

I’m illustrating with Grey so you know what I have added in this step

Glass Masking 02.png

This is what it looks like on a bead

Step 3 Black dots between white dots being melted.jpg

Repeat this with dots in between each of the white dots

I’m illustrating with Grey so you know what I have added in this step

Glass Masking 03.png

You should have something that looks like this (but on a round bead)

Glass Masking 04.png

And on an actual bead melted in:

Step 4 Black dots melted in.jpg

Add a white dot (using a stringer) on top of each of the black dots

Glass Masking 05.png

This is what it looks like on a bead

Step 5 Black dots on White dots.jpg

And melted in:

Step 6 Melted In.jpg

Add a black dot (using a stringer) on top of each of the white dots

Glass Masking 06.png

Add a black dot (using a stringer) on top of each of the original larger white dots

Glass Masking 07.png

Add a white dot (using a stringer) on top of each of the central black dots

Glass Masking 08.png

Add a small black dot (using a stringer) between each of the original large white dots

This is what it looks like on a bead

Step 7 More black dots.jpg

Stop, when you feel you have done enough

Glass Masking 09.png

Anyway, hopefully this shows the principle. Now you just have to accomplish this on a round bead.