Difference between revisions of "Glass Masking"
(Created page with 'Start with a base colour (black) and put on a set of contrast dots (white) framed|none Add a further set of base colour (black) in between the wh...') |
|||
Line 2: | Line 2: | ||
[[Image:Glass_Masking_01.png|framed|none]] | [[Image:Glass_Masking_01.png|framed|none]] | ||
+ | |||
+ | This is what it looks like on a bead | ||
+ | |||
+ | [[image:Step 1 Round black bead with white dots added.jpg]] | ||
Add a further set of base colour (black) in between the white dots. | Add a further set of base colour (black) in between the white dots. |
Revision as of 14:46, 19 November 2012
Start with a base colour (black) and put on a set of contrast dots (white)
This is what it looks like on a bead
Add a further set of base colour (black) in between the white dots.
I’m illustrating with Grey so you know what I have added in this step
Repeat this with dots in between each of the white dots
I’m illustrating with Grey so you know what I have added in this step
You should have something that looks like this (but on a round bead)
Add a white dot (using a stringer) on top of each of the black dots
Add a black dot (using a stringer) on top of each of the white dots
Add a black dot (using a stringer) on top of each of the original larger white dots
Add a white dot (using a stringer) on top of each of the central black dots
Add a small black dot (using a stringer) between each of the original large white dots
Stop, when you feel you have done enough
Anyway, hopefully this shows the principle. Now you just have to accomplish this on a round bead.