− | [[ | + | ASK [[glass]] used to be manufactured by [[Kugler]] and is currently out of production. It is still available in small quantities from a few stockists in a limited but bright colour palette. It is a type of silver rich [[soft glass]], compatible with [[Effetre]], [[Vetrofond]] and other [[CoE]] 104 Glass rods. |
+ | |||
+ | <!-- Please leave this at the bottom --> | ||
+ | [[Category:Types of Glass]] |