Line 183: Line 183:
 
|
 
|
 
|-
 
|-
 +
|060
 +
|cobalt blue
 +
|medium stiff glass
 +
|may pit if heated too quickly
 +
|-
 +
|064
 +
|black
 +
|medium stiff glass
 +
|
 +
|-
 +
|066
 +
|intense black
 +
|super dense colour
 +
|"crawls" when superheated - reacts with Effetre anice white
 +
 +
|-
 +
|068
 +
|pale rose
 +
|medium stiff glass
 +
|
 +
|-
 +
|069
 +
|electric yelow
 +
|medium stiff glass - striking
 +
|
 +
|-
 +
|070
 +
|uanium yellow
 +
|stiff glass
 +
|
 +
|-
 +
|071
 +
|yellow green
 +
|medium stiff glass - handpulled colour
 +
|
 +
|-
 +
|073
 +
|green apple
 +
|medium stiff glass
 +
|
 +
|-
 +
|076
 +
|red
 +
|stiff glass - striking
 +
|
 +
|-
 +
|080
 +
|pale lavender
 +
|medium stiff glass
 +
|
 +
|-
 +
|081
 +
|ark lavender
 +
|stiff glass - handpulled - dense colour
 +
|appears pale blue under U.V. light
 +
|-
 +
|082
 +
|blue pink (rosato)
 +
|medium stiff glass
 +
|
 +
|-
 +
|084
 +
|light grey
 +
|medium stiff glass
 +
|
 +
|-
 +
|088
 +
|dark grey
 +
|medium stiff glass
 
|}
 
|}
  

Revision as of 15:49, 15 November 2008

Effetre is glass made on the island of Murano, Venice, Italy. And is very popular with lampworkers partly due to the vast array of colours available.

Many stockists of Effetre glass rods use their own colour descriptions and stock numbers. The last 3 digits used by any stockist for their stock numbers will refer to the Effetre factory stock number.

Effetre colours and stock numbers

Transparent

Stock Number Colour Properties Reactions
004 clear melts quickly - may contain bubbles
005 super clear good for encasing silver glass - less scummy than 004
008 pale amber stiff glass
012 light topaz stiff glass
014 topaz reacts with silver glass - reacts with silver to produce organic effects
016 dark topaz (root beer) stiff glass
018 light brown stiff glass Reacts with iris gold frit
019 sage green reduces to terecotta in a propane rich flame
020 lightgrass green stiff glass may pit if heated too quickly
022 medium grass green stiff glass may pit if heated too quickly
023 green stiff glass may pit if heated too quickly
024 dark grass green medium stiff glass may pit if heated too quickly
025 olive
026 light teal
027 dark teal stiff glass - handpulled
028 light emerald green stiff glass
030 dark emerald green stiff glass - handpulled
031 pale emerald green stiff glass - handpulled
034 light aquamarine stiff glass - hardens quickly
035 antique aqua
036 dark aqua stiff glass may pit if heated too quickly
038 very pale aqua medium stiff glass may pit if heated too quickly
039 dark violet
040 light amethyst medium stiff glass
042 medium amethyst medium stiff glass
044 dark amethyst medium stiff glass
046 pale amethyst medium stiff glass
048 very pale blue gray medium stiff glass
049 straw yellow stiff glass - handpulled
050 pale blue medium stiff glass appears green as an encasement over ivory
052 light blue medium stiff glass may pit if heated too quickly
054 medium blue medium stiff glass may pit if heated too quickly
056 dark blue medium stiff glass may pit if heated too quickly
058 ink blue medium stiff glass - handpulled
060 cobalt blue medium stiff glass may pit if heated too quickly
064 black medium stiff glass
066 intense black super dense colour "crawls" when superheated - reacts with Effetre anice white
068 pale rose medium stiff glass
069 electric yelow medium stiff glass - striking
070 uanium yellow stiff glass
071 yellow green medium stiff glass - handpulled colour
073 green apple medium stiff glass
076 red stiff glass - striking
080 pale lavender medium stiff glass
081 ark lavender stiff glass - handpulled - dense colour appears pale blue under U.V. light
082 blue pink (rosato) medium stiff glass
084 light grey medium stiff glass
088 dark grey medium stiff glass