Difference between revisions of "Vetrofond"

From Fritipedia
Jump to navigationJump to search
Line 94: Line 94:
 
|
 
|
 
|-
 
|-
|}
+
|1060 cobalt blue
 
 
Opaque/pastels
 
{| class="wikitable"
 
|-
 
! Colour
 
! Properties
 
! Reactions
 
|-
 
|1204 white
 
 
|
 
|
 
|
 
|
 
|-
 
|-
|1206 anice white
+
|1064 black
 
|
 
|
 
|
 
|
 
|-
 
|-
|1208 silk white
+
|1068 pink
 
|
 
|
 
|
 
|
 
|-
 
|-
|1212 pea green
+
|1069 electric yellow
 
|
 
|
 
|
 
|
 
|-
 
|-
|1214 nile green
+
|1072 orange
 
|
 
|
 
|
 
|
 
|-
 
|-
|1216 grass green
+
|1076 red
 
|
 
|
 
|
 
|
 
|-
 
|-
|1218 dark grass green
+
|1080 pale lavender
 
|
 
|
 
|
 
|
 
|-
 
|-
|1220 periwinkle
+
|1082 lavender blue (alexandrite)
 
|
 
|
 
|
 
|
 
|-
 
|-
|1224 light sky blue
+
|1084 light brown
 
|
 
|
 
|
 
|
 
|-
 
|-
|1228 dark sky blue
+
|1086 medium brown
 
|
 
|
 
|
 
|
 
|-
 
|-
|1232 turquoise
+
|1088 dark brown
 
|
 
|
 
|
 
|
 
|-
 
|-
|1236 dark turquoise
+
|}
 +
 
 +
Opaque/pastels
 +
{| class="wikitable"
 +
|-
 +
! Colour
 +
! Properties
 +
! Reactions
 +
|-
 +
|1204 white
 
|
 
|
 
|
 
|
 
|-
 
|-
|1240 light lapis blue
+
|1206 anice white
 
|
 
|
 
|
 
|
 
|-
 
|-
|1242 lapis blue
+
|1208 silk white
 
|
 
|
 
|
 
|
 
|-
 
|-
|1246 cobalt blue
+
|1212 pea green
 
|
 
|
 
|
 
|
 
|-
 
|-
|1248 light grey
+
|1214 nile green
 
|
 
|
 
|
 
|
 
|-
 
|-
|1250 medium grey
+
|1216 grass green
 
|
 
|
 
|
 
|
 
|-
 
|-
|1255 flower pink
+
|1218 dark grass green
 
|
 
|
 
|
 
|
 
|-
 
|-
|1262 dark ivory
+
|1220 periwinkle
 
|
 
|
 
|
 
|
 
|-
 
|-
|1264 light ivory
+
|1224 light sky blue
 
|
 
|
 
|
 
|
 
|-
 
|-
|1268 pearl grey
+
|1228 dark sky blue
 
|
 
|
 
|
 
|
 
|-
 
|-
|1272 violet
+
|1232 turquoise
 
|
 
|
 
|
 
|
 
|-
 
|-
|}
+
|1236 dark turquoise
 
 
|1060 cobalt blue
 
 
|
 
|
 
|
 
|
 
|-
 
|-
|1064 black
+
|1240 light lapis blue
 
|
 
|
 
|
 
|
 
|-
 
|-
|1068 pink
+
|1242 lapis blue
 
|
 
|
 
|
 
|
 
|-
 
|-
|1069 electric yellow
+
|1246 cobalt blue
 
|
 
|
 
|
 
|
 
|-
 
|-
|1072 orange
+
|1248 light grey
 
|
 
|
 
|
 
|
 
|-
 
|-
|1076 red
+
|1250 medium grey
 
|
 
|
 
|
 
|
 
|-
 
|-
|1080 pale lavender
+
|1255 flower pink
 
|
 
|
 
|
 
|
 
|-
 
|-
|1082 lavender blue (alexandrite)
+
|1262 dark ivory
 
|
 
|
 
|
 
|
 
|-
 
|-
|1084 light brown
+
|1264 light ivory
 
|
 
|
 
|
 
|
 
|-
 
|-
|1086 medium brown
+
|1268 pearl grey
 
|
 
|
 
|
 
|
 
|-
 
|-
|1088 dark brown
+
|1272 violet
 
|
 
|
 
|
 
|
 
|-
 
|-
 
|}
 
|}
 +
 +
  
 
  Specials
 
  Specials

Revision as of 14:12, 14 November 2008

Vetrofond glass is manufactured in Italy. Many stockists of Vetrofond glass rods use their own colour descriptions and stock numbers. The last 4 digits used by any stockist for their stock numbers will refer to the Vetrofond factory stock number. Vetrofond colours and stock numbers

Transparent
Colour Properties Reactions
1004 clear Colours appear lighter encased in clear
1005 crystal clear good for encasing silver glass
1008 yellow
1012 light topaz
1014 topaz Reacts with DH psyche to give purples and blues
1020 light grass green
1022 grass green
1024 dark grass green
1026 teal
1028 light emerald green
1030 emerald green
1034 light aquamarine
1036 aquamarine (aqua)
1038 pale aquamarine (light aqua)
1040 light purple
1042 purple
1044 dark purple
1048 grey
1052 light blue
1054 blue
1058 intense blue
1060 cobalt blue
1064 black
1068 pink
1069 electric yellow
1072 orange
1076 red
1080 pale lavender
1082 lavender blue (alexandrite)
1084 light brown
1086 medium brown
1088 dark brown
Opaque/pastels
Colour Properties Reactions
1204 white
1206 anice white
1208 silk white
1212 pea green
1214 nile green
1216 grass green
1218 dark grass green
1220 periwinkle
1224 light sky blue
1228 dark sky blue
1232 turquoise
1236 dark turquoise
1240 light lapis blue
1242 lapis blue
1246 cobalt blue
1248 light grey
1250 medium grey
1255 flower pink
1262 dark ivory
1264 light ivory
1268 pearl grey
1272 violet


Specials
Colour Properties Reactions
1408 medium yellow
1412 dark lemon
1420 coral
1424 carrot red
1428 light red
1432 medium red
1438 red purple
1444 light brown
448 dark brown
1456 gold pink
1460 yellow ocher (wasabi)
Odd lots
Colour Properties Reactions
1801 cosmic storm
1802 apricot jam
1803 candy corn
1804 tomato soup
1805 orange dreamsicle
1806 smoke rings
1807 frog pond
1808 swamp moss
1809 jungle twilight
1810 lemongrass
1811 moon rock
1906 chardonnay
1909 transparent green odd
1910 transparent yellow odd
1911 silk white (opal white)
1912 olive green pastel
1917 Transparent amber (streaky amber)(antique amber)
1919 pale ivory
1922 transparent sage green
1925 transparent pale blue
1926 sea green (seafoam)
1927 ocean green
1931 river rock (brie)(avocado)
1932 fish pink
1933 pink no.3
1934 pink flower
1937 arancio perfecto
1938 pale aqua streaky
1939 intense tangerine
1943 orange sherbert (free range salmon pink)
1940 italian marble
1941 pineapple yellow
1942 watermelon (poppy)
1944 tangerine
1945 new white (custard)
1946 sunshine 1947 yellow ice (lemon ice)(belgian lace)
1948 banana cream
1949 lemon meringue
1951 transparent candy apple red
1952 violet odd (purplicious)
1954 cool white (odd cotton)
1955 seashell swirl
1957 orange punch
1958 pyjama blue
1960 light pink
1961 carrot red
1963 green tepenade
1964 pale avocado
1965 olive green
1966 dark olive green
1967 quartz grey
1968 slate blue
1969 pearl grey
1970 transparent streaky sapphire
1975 midnight blue
1976 key lime green
1977 parrot green
1978 transparent crystal green
1980 light streaky brown
1981 streaky brown
1982 dark streaky brown
1983 pale ocean blue
1984 pale moss agate
1985 moss agate
1986 lichen
1987 dark lichen
1988 pale crystal green
1989 transparent odd topaz
1990 honey crunch
1991 marbled avocado
1992 banana
1993 sweet lime (red jasper)
1994 strawberry sweet (dark red jasper)