Difference between revisions of "Strain point"

From Fritipedia
Jump to navigationJump to search
Line 5: Line 5:
  
 
==Effetre glass==
 
==Effetre glass==
The annealing temp is between 493C - 520C but the strain point is 448C
+
The [[annealing range]] is between 493C - 520C and the strain point is 448C
  
 
==Bullseye==
 
==Bullseye==
 
The annealing temp is 504C and strain point is 437C
 
The annealing temp is 504C and strain point is 437C

Revision as of 18:06, 12 November 2008

This is the temperature at which the molecules in the glass stop flowing and moving. Below this point if the bead has not been annealed correctly these stresses will remain in the glass. (unless the glass is then subsequently annealed).

The strain point varies for each glass depending on the manufacturer, elements contained within the glass and the coefficiency of the glass

Effetre glass

The annealing range is between 493C - 520C and the strain point is 448C

Bullseye

The annealing temp is 504C and strain point is 437C