RLBrown

Hi

I was just wondering if anyone has used the warm glass printable decals with a Dell laser printer?

The listing says HP and Canon, but we've got a Dell.

TIA

Zeldazog

It needs iron content in the printing product to work, so if you can find a materials spec for the toner cartridge, does that give any info?

RLBrown

Ah. Now I know what to look for... Thanks


I've just googled the MSDS for my printer and it appears not :-(

Oh well still other options. And lots of other techniques to try.