Main Menu

CIM dirty martini

Started by micpru, May 12, 2013, 11:24:04 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

micpru

Everywhere seems to be out of CIM dirty martini. Can anyone suggest a similar coloured glass? X
Michaela x

Kaz

Effetre green tea.
CIM cardamom -  a bit greener.
CIM linen - similar tone.
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

micpru

Michaela x

Shirley

Depending on what you're doing to it and using it with, Effetre Copper Green can work in a similar way
Val Cox Frit - Thai and Bali Silver