Started by Sam, September 03, 2009, 10:03:16 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Sam

Hi Guys,


Just wondering if anyone knows how to use a cabachon mandrel ???



Thanks


Sam ;D

sarah t

never used one myself but i think lorna demonstated on one at julies ??.......could be wrong but wasnt that the thing she did the 'twirl it ' and the glass will flow to the edges'.. ??

pixiewillow

Lol yup that was it   ;D


Okay here's what i do....

1) get your mandrel really really hot while you are getting a really good sized gather of glass on the end of your rod.

2) Let the gather drip onto the little bobbly sticky up thing on the mandrel (oooay technical terms here lol!)

3) then build up your glass ontop of that blob kinda like a mr whippy  ;)

4) when you have a good amount on get all the glass really hot so it starts to move freely but not too runny

5) take the mandrel out of the flame and with the mandrel completely vertical gently spin backwards and forwards between your thumb and forefinger, this will displace the glass evenly into a lovely round cab (in theory!!)

hope This helps and I haven't confused you lol!!

lorna XX
www.pixiewillow.etsy.com
www.pixiewillowdesigns.com
A mans idea of multi tasking is breathing & blinking at the same time.

Sam

Thanks very much Pixie.

I would never have worked that one out in a million years ;D

Okay, you know my next question don't you?

Where do you get them?

I did see that Martin had one size on his site but it looks a litle big for me :)


Thanks again,


Sam.

Donna@Rockin' Beads

Aha, that's what I've been doing wrong - I've been pressing and marvering to try to get a nice shape. I will try some twirling from now on...
Thanks Lorna