Did I leave these lil fellas in the Etchall' too long ???

Started by Vicki.White, May 18, 2009, 12:29:08 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Vicki.White



and is there anything I can do to get those stupid white blotches off???

Silly me!!!!

xxx ::)

Sulis (Hazel)

I dunno Vicki, but it MAY just be worth a try giving them a little soak in Cilit Bang lime & grime version. Just a thought. Last resort and all that!

Good luck!!  :)
Hazel x

Vicki.White

Oooh, what I good idea... I would have never thought of that! Cheers... will report back  :P hehe
x

Kaz

She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

pixiewillow

Quote from: Kaz on May 18, 2009, 07:24:48 AM
Hot water, washing up liquid and a nail brush.
Kazx

Yup was gonna say the same, its just residue of acid.
I have a spare tooth brush I scrub mine with  ;)
www.pixiewillow.etsy.com
www.pixiewillowdesigns.com
A mans idea of multi tasking is breathing & blinking at the same time.

pixiewillow

www.pixiewillow.etsy.com
www.pixiewillowdesigns.com
A mans idea of multi tasking is breathing & blinking at the same time.

Trudi

Also after I've dipped in etch all - I then plunge them in warm water with bicarb of soda - helps to neutralise the acid!


TiaraHelen

Even after mine look ok after rinsing etc sometimes they get a sort of bloom on them.  I followed Corina's tip of rolling them in my palms after I've rubbed in a small dab of handcream.  It gives them a lovely glow (and good for your hands too!).
Helen x

Even after all this time, the sun never says to the earth "you owe me".

Wishing Wells Glass

I use a teeny amount of beeswax :)  (although the hand cream tip is probably just as effective!)

x

Trudi

Quote from: Wishing Wells Glass on May 18, 2009, 04:01:05 PM
I use a teeny amount of beeswax :)  (although the hand cream tip is probably just as effective!)

x