At What Rate does a Kiln Cool Down?

Started by Stacy, February 19, 2008, 12:47:30 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Sal

Oooh-that sounds really exciting! (I still think you should show us some pictures  ;D)

Zeldazog

I read you can do it with a terracotta plant pot - you can get those tiny ones and drill holes in the bottom - have seen the mesh ones too - what a shame Stacy!

I really want to try one of these, gonna have to raid a college or uni kiln, methinks.........

julieHB

wow, that's fantastic!!  Never heard of a pot melt, but it sounds delicious.  Might have to try that some day!!  Sorry that it all melted together, Stacy!
Julie xx

                           My Webbie - My Flickr

Stacy

Quote from: zeldazog on February 19, 2008, 09:29:40 PM
I read you can do it with a terracotta plant pot - you can get those tiny ones and drill holes in the bottom - have seen the mesh ones too - what a shame Stacy!

I really want to try one of these, gonna have to raid a college or uni kiln, methinks.........

Ohh I've got one of those - Gonna have to give that a go today or tomorrow! thanks Dawn!

Dennis Brady

A "shelf melt" is when you pile up glass on the kiln shelf and fire it to all melt together.

A "pot melt" is when you suspend a pot (like a flower pot) over the kiln shelf and let the molten glass run out through the hole in the pot.

A "screen melt" is when you suspend screen over the kiln shelf and let the molten glass melt through the screen.  Here's some examples of screen melts.
http://www.vicartglass.com/products/screen%20melts/screenmelts.html