Fusion 7 Firing schedules

Started by fleurbrawl, June 15, 2009, 09:50:24 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

fleurbrawl

Finally got round to picking up a Fusion 7.
Does anyone have any firing schedules they don't mind sharing?
I've got some base ones from the web and old ones that used to work in an SC2.
Kays' OH :)


2B or not 2B, that is the pencil.

Zeldazog

Just seen this, doesn't the Fusion have the same controller as the SC2?

Remember that the larger/thicker the piece, the slower you go.

fleurbrawl

Yeah, very similar.
I ended up using the same schedules again and adjusting them slightly for the kiln over a few goes.
Kays' OH :)