Hollow beads and bead poo

Started by wendy j, May 31, 2009, 10:22:50 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

wendy j

OK,  maybe just a big trapped air bubble  ::),  but how do I get rid of the bead release that flaked off from the mandrel as it was pulled out?    Ive got the bead soaking in water at the moment shaking it every time I go past hoping that will break it down .
Hope some one know the answer,
Wendy

saffie

nope just keep on shaking very vigorously!!! it will break up and come out eventually
xx

TiaraHelen

If it's not dissolving, can you gently poke it inside the bead with a mandrel?
Helen x

Even after all this time, the sun never says to the earth "you owe me".

Pat from Canvey

Cillit Bang or Grime and Lime. Let the bead soak for a while.

hollergrafik

I shake mine to break it up then blow through the holes.

♥♥Tan♥♥


Sulis (Hazel)

Quote from: Tan on May 31, 2009, 05:31:46 PM
BLow job for me too!

Oh Tan, what would we do without you?!  ;D ;D ;D  x
Hazel x

Lloki

Cerri

Margram

Yes, we'd all be completely sniggerless.

Marg x
Marg x  Etsy Flickr My blog