Respiratory protection

Started by Annelyse, June 18, 2007, 03:03:42 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Annelyse

Does anybody know what type of filters we are supposed to use for protection against metal fumes and enamels? Is P1, P2 or P3?
I was told a few days ago and I can't remember now ???

Thank you

Annelyse

Buzzybead

P3!! Apparently B&Q make a really good mask with changeable filters for about £35.00. MUCH better than the disposables I bought.

Caroline

they don't at the B&Q in Aberdeen! I've already checked!



Annelyse

Thanks for the reply! How could I not remember ...It must be all the lead getting to my brain... :-[ ;)

I looked at both B&Q in Aberdeen and no...nothing :(