How to fuse with gold/silver lettering

Started by Flowers, March 01, 2021, 01:51:29 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Flowers

Hi I hope you are all well.
I often see beautiful plates and dishes with gold and/or silver writing fused on or into them
I would love to have a try and saw one advertised recently on Etsy where they say they use 23K gold lettering.  How is this done?  Where does one buy such a thing? If anyone could shed some light on the technique, what sort of gold and silver is used and where to purchase such products that would be super 🙂
Many thanks

Nicknack

Warm Glass sell a gold pen, but it's quite expensive.

Flowers


Flowers

I can't find a gold pen on their website do you mean the Glassline colours?

Nicknack

I can't find it there now, either, sorry. Try Bath Potters, they do a metallic lustre. The gold one should be fired  last, at 500-600 C.  You use a paintbrush. Hope that helps.

Nick

beadammed

I've seen something on you tube where 24k gold liquid is put in a little cup thing attached to a pen type holder with a fine nib for writing. I think it's mostly used by potters.  I'll see if I can find it again.
Geraldine
Geraldine
www.etsy.com/uk/shop/strikingglassstudios

Flowers

Thank you all so much.  I wish I couldl find a gold decal paper that would probably work but haven't managed to yet!