Is this air bubble ok?

Started by Amber, October 14, 2009, 08:42:13 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Amber



This bead has a pointy air bubble right on the core...I just wanted to know whether it is could cause problems (cracking etc)? I made it several months ago and it seems ok so far - but I obviously don't want to sell it if it's likely to fall to pieces or something!

Any idea?

Dragonfire Glass

neat effect - can you do it again?  :D

sea-thistle


Kaz

Looks like the answer is that no-one knows! :D
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

llewennog

I'd say that if it been Annealed properly then you've relieved all the potential stress within, that area and not to worry about it,  I use Air bubbles quite a lot in dot implosions and ive not had one crack , even when they've not been annealed until sometime after.