Galaxy Bead Tutorial

Started by Veebee, June 24, 2011, 07:51:12 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Veebee

Linda, did you burn off the reduction before encasing? I'm on a Hot head and tend to get that effect when there is too much redution on the surface before encasing.
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Madam Steph

Aaaaaaaaaaaaaaaaaaaaarrrrrrghhhhhhhhhh!!!!!!!!!
No, Vee.
I thought I followed the instructions so well. GRRRRRRR!!!

<<<Looking extremely sheepish

Veebee

To be fair, they are a bit squished up together but I didn't want to take up too much forum space  ;D
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Madam Steph

No.....they were fine.
It was me.

I was trying to torch and read (and I thought I could multitask)  :P

Soon as my Cricket arrives, and it should be on Tuesday, it will be one of the first things I will retry.

I don't like stuff to beat me

Kaz

Here's one from me
Added silvered ivory ends and some murrini (new Buttermint!)

IMG_1936 by Kaz ~ CheekyCherubDesigns, on Flickr
Thanks for this Vicki!
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Veebee

OMG that is stunning Kaz!!  :o
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Lush!

Quote from: Veebee on June 26, 2011, 05:25:43 PM
OMG that is stunning Kaz!!  :o

Yup!!

Great tut, Vee. We did something very similar on the Andrea Guarino class with the clear trails that turn blue.


www.lushlampwork.etsy.com

Madam Steph


Margram

Ooh, Kaz - lovely! :)

This is one I made back in the spring - purple red and silver leaf: it has a bit of the blue halo effect

by Rosyglowglass, on Flickr
and this one I made yesterday with the clear stringer and encasing - much more blue, and I like the veining

Blue red heart  3cm tall by Rosyglowglass, on Flickr
Took this from the side to show the effect of the criss-cross clear stringer

by Rosyglowglass, on Flickr
Marg x  Etsy Flickr My blog

poledra1958

Great tutorial,  will print off and try soon.


HH on Bulk,

Veebee

Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

awrylemming

I've had a go with the howaco blue silver just to see if it makes a difference.  *sigh*  I'm keeping my fingers crossed.

Kathy

Soooooooooooooo pretty - gonna try this today! (Fingers, legs, and everything else crossed)!!!   :) :) :)

Sarah9959

What a fantastic tutorial, really well written and explained - thanks very much   :) :) :)

Kathy

Ahhhhh nothing but poo-brown on my first attempt! Will try again later today :)