Frit-Happens !

Lampwork => Other COE Glass => Topic started by: catriona on March 06, 2008, 09:28:47 PM

Title: Bullseye Glass
Post by: catriona on March 06, 2008, 09:28:47 PM
Can anyone help me I,ve just bought some bullseye glass and was wondering if it would be ok to use beadie sams frit with it .the glass is coe90 and i noticed the frit is 89 to 96 .
xxcatxx
Title: Re: Bullseye Glass
Post by: Josephine on March 06, 2008, 09:30:39 PM
Should be ok. Most of us use it with 104 coe glass so  the difference is actually less with the bullseye.
Title: Re: Bullseye Glass
Post by: *rowanberry* on March 07, 2008, 11:17:53 AM
I use bullseye now and again and the frits were no problem.
Title: Re: Bullseye Glass
Post by: catriona on March 07, 2008, 01:26:19 PM
Thanks girls will now give it a go .
xxcatxx