I have now sent a fair bit of this out and would love to see what you do with it.
I have kept a pack of each for myself for Christmas and will be using the time between now and New Year to have a damn good mess with it!
Kazx
Ekho frit over clear with silver foil melted in
(http://farm6.static.flickr.com/5083/5342017077_3d143682f2.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5342017077/)
IMG_0253 (http://www.flickr.com/photos/cheekycherubdesigns/5342017077/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
Triton frit over transparent light purple with silver foil melted in
(http://farm6.static.flickr.com/5207/5342627066_bb54f91402.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5342627066/)
IMG_0251 (http://www.flickr.com/photos/cheekycherubdesigns/5342627066/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
Gaia frit over clear with silver foil melted in and then sprinkled with Multicolour Dark powder
(http://farm6.static.flickr.com/5089/5342627266_e69ecf4b52.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5342627266/)
IMG_0252 (http://www.flickr.com/photos/cheekycherubdesigns/5342627266/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
Psyche core with terranova 2 frit encased in 006
(http://farm6.static.flickr.com/5001/5342016055_ccca4e33d9.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5342016055/)
IMG_0241 (http://www.flickr.com/photos/cheekycherubdesigns/5342016055/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
Terranova 2 core with Luna 2 frit encased in 006. The spacers are terranova 2 with a sprinkling of Luna 2 frit
(http://farm6.static.flickr.com/5162/5342626176_e9da477b4f.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5342626176/)
IMG_0239 (http://www.flickr.com/photos/cheekycherubdesigns/5342626176/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
White core encased in ink blue with Triton frit and encased in 006
(http://farm6.static.flickr.com/5042/5342626474_a18a1db0fb.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5342626474/)
IMG_0244 (http://www.flickr.com/photos/cheekycherubdesigns/5342626474/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
These are psyche frit (that I got from Martin probably with my first glass order) and shows what you can get when you don't really know what you're doing, playing with a hothead and repeatedly heating it to stretch the bead and most likely not reducing at the very end. I love them, the first is on a base of white, the second on black.
(http://farm5.static.flickr.com/4027/4329397061_722873df4a_m.jpg) (http://www.flickr.com/photos/helenpetersbeads/4329397061/)
Dinosaur bone (2) (http://www.flickr.com/photos/helenpetersbeads/4329397061/) by HelenPetersBeads (http://www.flickr.com/people/helenpetersbeads/), on Flickr
(http://farm5.static.flickr.com/4006/4329407447_f8965bd3f7_m.jpg) (http://www.flickr.com/photos/helenpetersbeads/4329407447/)
Dinosaur bone 1 (http://www.flickr.com/photos/helenpetersbeads/4329407447/) by HelenPetersBeads (http://www.flickr.com/people/helenpetersbeads/), on Flickr
Vetrofond black with Luna 2 frit and pure silver wire encased in 006.
(http://farm6.static.flickr.com/5168/5359711767_44c2c2be7c.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5359711767/)
Dreamy Planets (http://www.flickr.com/photos/cheekycherubdesigns/5359711767/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
Wow, missed this completely! Rachel, that is one beautiful bead! I'm in agreement about Kaz's terra frit bead and I love the dino bones too!
These are from my first test session:
Electra over 006, encased in 006:
(http://i630.photobucket.com/albums/uu26/veebeads/beads%202011/electra2comp.jpg)
Terra over 006 encased in 006:
(http://i630.photobucket.com/albums/uu26/veebeads/beads%202011/terraComp.jpg)
my first beads on this forum!:
triton over stiking red encrased in oo6
(http://www.mijnalbum.be/Foto-LJDB4DBS-D.jpg)
and triton over 006 encrased in oo6:
(http://www.mijnalbum.be/Foto-6BCT3ZX3-D.jpg)